SAE J431 automotive gray cast iron, SAE grade G4000
Subcategory: Gray Cast Iron; Metal
Key Words: UNS F10008, ferritic, pearlitic, soft iron castings
Material Notes: If Carbon or Silicon is on the high % range end, the other should be on the low % end. Properties determined from as-cast test bar 30.5 mm diameter. Pearlitic microstructure. Applications include diesel engine castings, liners, cylinders, and pistons. 1180 kg minimum transverse load, 6.9 mm minimum deflection.