SAE J431 heavy duty automotive gray cast iron, SAE grade G3500c
Subcategory: Gray Cast Iron; Metal
Key Words: UNS F10011, ferritic, pearlitic, soft iron castings
Material Notes: If Carbon or Silicon is on the high % range end, the other should be on the low % end. Alloying elements not listed may be required. Properties determined from as-cast test bar 30.5 mm diameter. Microstructure: size 3 to 5 type A graphite in a matrix of lamellar pearlite containing not more than 5% free ferrite or free carbide. Applications include brake drums for extra heavy duty service. 1090 kg minimum transverse load, 6.1 mm minimum deflection.