Oxygen-free silver-bearing Copper, UNS C10500, H02 Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: AMSIL Copper; Oxygen-free Silver-Copper; ASTM-B-152, QQ-C-576, C103
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: auto gaskets, radiators, busbars, conductivity wire, contacts, radio parts, winding, switches, terminals, commutator segments, chemical process equipment, printing rolls, clad metals, printed circuit foil. Test specimens: flat product - 1 mm thickness. 8 oz/ton Ag (UNS C10400), 10 oz/ton Ag (UNS C10500), 25 oz/ton Ag (UNS C10700).
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|