Oxygen-free low phosphorus Copper, UNS C10800, OSO50 Temper flat products, tubing
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: AMAX-LP Copper
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: refrigerators, air conditioners, gas and heater lines, oil burner tubes, brewery tubes, condenser and heat exchanger tubes, dairy and distiller tubes, pulp and paper lines, tanks, air, gasoline, hydraulic and oil lines. Test specimens: flat products - 6mm thickness and tubing - 25mm OD x 1.65 mm wall thickness.
| Available Properties |
- Density
- Hardness, Rockwell F
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|