|   Oxygen-free low phosphorus Copper, UNS C10800, H04 Temper flat products  Subcategory: Copper Alloy; Nonferrous Metal Key Words: AMAX-LP Copper Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.
 Applications: refrigerators, air conditioners, gas and heater lines, oil burner tubes, brewery tubes, condenser and heat exchanger tubes, dairy and distiller tubes, pulp and paper lines, tanks, air, gasoline, hydraulic and oil lines.Test specimens: flat products - 25mm thicknesses. 
| | 
    | Available Properties |  
    | DensityHardness, Rockwell BHardness, Rockwell FTensile Strength, UltimateTensile Strength, YieldElongation at BreakModulus of ElasticityPoissons RatioMachinabilityShear ModulusShear StrengthElectrical ResistivityCTE, linear 20°CCTE, linear 100°CCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting PointSolidusLiquidusAnnealing TemperatureHot-Working Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |