Electrolytic tough pitch Copper, UNS C11000, H02 Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: ASTM-B-152, QQ-C-576, CDA 110 ETP, C101, ISO Cu-ETP
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: downspouts, gutters, roofing, gaskets, auto radiators, busbars, nails, printing rolls, rivets, and radio parts. Test specimens: flat products - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Coefficient of Friction
- Coefficient of Friction, Static
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Softening Point
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,