|   Copper, UNS C12000, UNS C12100  Subcategory: Copper Alloy; Nonferrous Metal Key Words: ISO Cu-DLP, CEN CW023A Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.
 Applications: busbars, electrical conductors, tubular bus, and applications requiring welding or brazing.Available as flat products, tube, pipe. UNS C12000 0.008 P and 4 oz/ton Ag. 
| | 
    | Available Properties |  
    | DensityTensile Strength, UltimateTensile Strength, YieldElongation at BreakMachinability
 | 
 | 
 |  | | 
    | Property Data |  
    | 