|   Fire-refined tough pitch with silver Copper, UNS C12500, UNS C12700, UNS C12800, UNS C12900, UNS C13000, OSO50 Temper rod, shapes  Subcategory: Copper Alloy; Nonferrous Metal Key Words: C104, Tough pitch, non-arsenical copper, ISO Cu-FRTP, CEN CW006A Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.
 Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables and tubes, klystrons, microwave tubes, and rectifiers.Test specimens: rod - 25mm diameter and shapes - 13mm diameter. 8 oz/ton Ag (UNS C12700), 10 oz/ton Ag (UNS C12800), 16 oz/ton Ag (UNS C12900), 25 oz/ton Ag (UNS C13000). 
| | 
    | Available Properties |  
    | DensityHardness, Rockwell FTensile Strength, UltimateTensile Strength, YieldElongation at BreakMachinabilityShear StrengthElectrical ResistivityCTE, linear 20°CCTE, linear 100°CCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting PointLiquidusAnnealing TemperatureHot-Working Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |