Cadmium Copper, UNS C16200, Half Hard (25%) Temper rod
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: C108, ISO CuCd1, A1/3, cadmium bronze, copper-cadmium
Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: trolley wire, heating pads, electric-blanket elements, spring contacts, railbands, high-strength transmission lines, connectors, cable wrap, switch gear components and wave guide cavities. Test specimen: rod - 13mm diameter; half hard(25%) temper.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|