Chromium Copper, UNS C18400, TD04 Temper tube
Subcategory: Copper Alloy; Nonferrous Metal
Close Analogs: UNS C18400, UNS C18500
Key Words: CDA 182, CC101, ISO CuCr1, CEN CW105C, A2/1
Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot workability. Applications: resistance welding electrodes, seam welding wheels, switch gear, electrode holder jaws, cable connectors, current carrying arms and shafts, circuit breaker parts, molds, spot welding tips, flash welding electrodes, electrical and thermal conductors requiring strength, switch contacts. Test specimen: tube - 31.8mm OD x 5.4mm wall thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
- Solution Temperature
- Aging Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|