Beryllium Copper, UNS C17200, TF00 Temper Strip
Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy
Key Words: BeCu; CDA 172, CB101, ISO CuBe2, CEN CW101C, A4/2, beryllium bronze; Alloy 25
Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping. Applications: springs, flexible metal hose, Bourdon tubing, bellows, clips, washers, retaining rings, and other parts subject to severe forming conditions but require high strength, anelasticity, and fatigue and creep resistance; in parts that require high strength or wear resistance along with good electrical conductivity and/or magnetic characteristics such as navigational instruments, non-sparking safety tools, firing pins, bushings, valves, pumps, shafts, and rolling mill parts. Solution treated and aged 3 hours at 315°C.
| Available Properties |
- Density
- Hardness, Rockwell C
- Hardness, Rockwell HR30N
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Processing Temperature
- Annealing Temperature
- Solution Temperature
- Aging Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|