Copper-Cobalt-Beryllium alloy, UNS C17500, TF00 Temper strip, rod, bar, plate, tubing, forged products
Subcategory: Copper Alloy; Nonferrous Metal; Beryllium Alloy
Key Words: BeCu; low beryllium copper, C112, ISO CuCo2Be, CEN CW104C, A3/1
Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: fuse clips, fasteners, springs, switch and relay parts, electrical conductors, welding equipment. TF00 temper strip, rod, bar, plate, tubing, and forged products.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
- Processing Temperature
- Solution Temperature
- Aging Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|