Copper-Nickel-Phosphorus alloy, UNS C19000
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: springs, clips, electrical connectors, power tube and electron tube components, high-strength electrical components, bolts, nails, screws, cotter pins, and parts requiring some combination of high-strength, high electrical or thermal conductivity, high resistance to fatigue and creep, and good workability. Available as flat products, rod, wire.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|