Copper-Nickel-Phosphorus-Tellurium alloy, UNS C19100
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Good to excellent corrosion resistance. Good hot and cold workability. Applications: forgings and screw machine parts requiring high strength, hardenability, extensive machining, corrosion resistance, copper color, good conductivity, or a combination of these: bolts, bushings, electrical connectors, gears, marine hardware, nuts, pinions, tie rods, turnbuckle barrels, welding torch tips. Available as flat products.