Red Brass, UNS C23000 (230 Brass), H06 Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: CDA 230, CZ102, ISO CuZn15, CEN CW502L, gilding metal, 85/15 brass
Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: weather-stripping, conduit, sockets, fasteners, fire extinguishers, condenser and heat exchanger tubing, plumbing pipe, radiator cores. Test specimen: flat products - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact
- Izod Impact
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Magnetic Susceptibility
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
- Velocity of Sound
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|