Brass, Low, CDA 240
Subcategory: Copper Alloy; Zinc Alloy; Nonferrous Metal
Key Words: ASTM B134, QQ-W-321
Material Notes: All values may vary dependant on specific design and usage Capabilities: - Wire
- Ribbon
- Square
- Insulated
- Plated
Information provided by California Fine Wire.
| Available Properties |
- Density
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Modulus of Elasticity
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Magnetic Susceptibility
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Melting Point
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
- Magnetic
- Temperature Coefficient of Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|