Copper, UNS C27000 (Yellow brass), H10 Temper wire
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: ASTM B36, ASTM B587, SAE J461, SAE J463, MIL-W-6712, CDA 268, ISO CuZn33, CEN CW506L, 67/33 brass, ISO CuZn35, 65/35 brass
Material Notes: Fair to excellent corrosion resistance. Excellent cold workability. Applications: radiator cores and tanks, flashlight shells, lamp fixtures, fasteners, locks, hinges, plumbing accessories, pins, rivets. Test specimen: wire - 2mm diameter.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|