Low-leaded brass tube, UNS C33000
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: CDA 330
Material Notes: Fair to excellent corrosion resistance. Combines good machinability and excellent cold workability. Fabricated by forming and bending, machining, piercing and punching. Applications: pump and power cylinders and liners, ammunition primers, plumbing accessories. Available as tube.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- CTE, linear 250°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|