Medium-leaded brass, UNS C34000, OSO25 Temper wire
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: 340 brass, CZ118, ISO CuZn35Pb1, CEN CW600N
Material Notes: Please Note: Zinc content is calculated as a remainder. Fair to excellent corrosion resistance. Fabricated by blanking, heading and upsetting, machining, piercing and punching, roll threading and knurling, stamping. Applications: couplings, free machining screws and rivets, gears, nuts, or tire valve stems. Test specimen: wire - 2mm diameter.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|