Medium-leaded brass, UNS C35000, H01 Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: CZ129, ISO CuZn37Pb1, ISO CuZn38Pb1, CEN CW605N, CEN CW607N
Material Notes: Fair to excellent corrosion resistance. Fair cold workability, poor hot formability. Applications: bearing cages, book dies, clock plates, engraving plates, gears, hinges, hose couplings, keys, lock parts, lock tumblers, meter parts, nuts, sink strainers, strike plates, templates, type characters, washers, wear plates. Test specimen: flat product - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|