Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 18%) Temper 50 mm rod
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: free cutting, FC, CDA 360, CZ124, ISO CuZn36Pb3, CEN CW603N, FED QQ-B-626 (discontinued), ASTM-B121, ASTM-B36, ASTM-B16/B16M, ASTM-B124
Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Fabricated by machining, roll threading and knurling. Applications: gears, pinions, automatic high-speed screw machine parts. Test specimen: rod - 50mm diameter.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|