Free-Cutting Muntz Metal, UNS C37000, H80 (Cold Drawn 35%) Temper 38 mm tube
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Combines good machinability with excellent hot formability. Applications: automatic screw machine parts. Test specimen: tube - 38mm OD x 3mm wall thickness.
| Available Properties |
- Density
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|