Phosphorized Admiralty Copper, UNS C44500, OSO60 (0.015mm) Temper strip
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: Inhibited Admiralty Metal, Admiralty Brass, CDA 443, CZ111, ISO CuZn28Sn1As
Material Notes: Good to excellent corrosion resistance. Excellent cold workability for forming and bending. Applications: condenser, evaporator and heat exchanger tubing, condenser tubing plates, distiller tubing, ferrules. Test specimen: strip - 1mm diameter.
| Available Properties |
- Density
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Charpy Impact
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|