Medium leaded naval brass, UNS C48200, H01 (8%) Temper 25 mm rod
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: ISO CuZn37Pb1Sn1, ISO CuZn36Sn1Pb, CEN CW712R, CEN CW714R
Material Notes: Fair to excellent corrosion resistance. Good hot workability for hot forging, pressing, and machining operations. Applications: marine hardware, screw machine products, valve stems. Test specimen: rod - 25mm diameter.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|