Copper, UNS C51100, OSO15 Temper strip
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: PB101, ISO CuSn4
Material Notes: Good to excellent corrosion resistance. Excellent cold workability. Applications: bridge bearing plates, locator bars, fuse clips, sleeve bushings, springs, switch parts, truss wire, wire brushes, chemical hardware, perforated sheets, textile machinery, welding rod. Test specimen: strip - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell F
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|