Phosphor bronze 10% D, UNS C52400, H02 Temper wire
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Material Notes: Good to excellent corrosion resistance. Good cold workability for blanking, forming and bending, shearing. Applications: heavy bars and plates for severe compression, bridge and expansion plates and fittings, articles requiring good spring qualities, resiliency, fatigue resistance, good wear and corrosion resistance. Trace content of Phosphorus.Test specimen: wire - 2mm diameter.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|