8% Aluminum Bronze, UNS C61000
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: CDA 610
Material Notes: Good to excellent corrosion resistance. Good hot and cold workability. Applications: bolts, pump parts, shafts, tie rods, overlay on steel for wearing surfaces. Properties typical for rod, 25mm in diameter.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|