Nickel Aluminum Bronze, UNS C63200
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: Copper, CDA 632
Material Notes: Good to excellent corrosion resistance. Good hot formability. Fabricated by hot forming and welding. Applications: nuts, bolts, structural pump parts, shafting requiring corrosion resistance. Available as rod, bar, and forgings.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Poissons Ratio
- Charpy Impact
- Izod Impact
- Machinability
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|