Copper, UNS C63600, H01 Temper rod
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Good to excellent corrosion resistance. Excellent cold workability, fair hot formability. Fabricated by cold heading. Applications components for pole-line hardware, cold headed nuts for wire and cable connectors, bolts and screw products. Test specimen: rod - 14mm diameter.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- CTE, linear 250°C
- Thermal Conductivity
- Melting Point
- Liquidus
- Hot-Working Temperature
|
|
|
|