Low-silicon bronze B, UNS C65100, H04 (60%) Temper 11 mm wire
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: CDA 651, ISO CuSi1, CEN C115C
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Fabricated by forming and bending, heading and upsetting, hot forging and pressing, roll threading and knurling, squeezing and swaging. Applications: hydraulic pressure lines, anchor screws, bolts, cable clamps, cap screws, machine screws, marine hardware, nuts, pole-line hardware, rivets, U-bolts, electrical conduits, heat exchanger tubing, welding rod. Test specimen: wire - 11mm diameter.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|