Herculoy®, High-Silicon Bronze A, UNS C65500, H06 Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal; Bronze
Key Words: HCDA 655, CS101, ISO CuSi3Mn1, CEN CS101, copper-silicon, silicon bronze
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Fabricated by blanking, drawing, forming and bending, heading and upsetting, hot forging and pressing, roll threading and knurling, shearing, squeezing, and swaging. Applications: hydraulic pressure lines, anchor screws, bolts, cable clamps, cap screws, machine screws, marine hardware, nuts, pole-line hardware, rivets, U-bolts, electrical conduits, heat exchanger tubing, welding rod, propeller shafts. Test specimen: flat products - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|