|   Herculoy®, High-Silicon Bronze A, UNS C65500, H02 Temper wire  Subcategory: Copper Alloy; Nonferrous Metal; Bronze Key Words: HCDA 655, CS101, ISO CuSi3Mn1, CEN CS101, copper-silicon, silicon bronze Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Fabricated by blanking, drawing, forming and bending, heading and upsetting, hot forging and pressing, roll threading and knurling, shearing, squeezing, and swaging.
 Applications: hydraulic pressure lines, anchor screws, bolts, cable clamps, cap screws, machine screws, marine hardware, nuts, pole-line hardware, rivets, U-bolts, electrical conduits, heat exchanger tubing, welding rod, propeller shafts.Test specimen: wire - 2mm diameter. 
| | 
    | Available Properties |  
    | DensityTensile Strength, UltimateTensile Strength, YieldElongation at BreakModulus of ElasticityPoissons RatioMachinabilityShear ModulusShear StrengthElectrical ResistivityCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting PointSolidusLiquidusAnnealing TemperatureHot-Working TemperatureRecrystallization Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |