Aluminum Brass Arsenical, UNS C68700
Subcategory: Copper Alloy; Nonferrous Metal; Brass
Key Words: CDA 687, CZ110, ISO CuZn20A12As
Material Notes: Good to excellent corrosion resistance. Excellent cold workability for forming and bending. Applications: condenser, evaporator and heat exchanger tubing, condenser tubing plates, distiller tubing, ferrules. Available as tube.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
|
|
|
|