Alcoloy Copper, UNS C68800, O50 Temper strip
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Good to excellent corrosion resistance. Excellent hot and cold formability. Fabricated by blanking, drawing, forming and bending, shearing and stamping. Applications: springs, switches, contacts, relays, drawn parts. Test specimen: strip - 1mm thickness.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Magnetic Permeability
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|