|   Silicon Red Brass, UNS C69400, O60 Temper 51 mm rod  Subcategory: Copper Alloy; Nonferrous Metal; Brass Key Words: CDA 694 Material Notes: Good to excellent corrosion resistance. Excellent hot formability for fabrication by forging, screw machine operations.
 Applications: valve stems where corrosion resistance and high strength are critical.Test specimen: rod - 51mm diameter. 
| | 
    | Available Properties |  
    | DensityHardness, Rockwell BTensile Strength, UltimateTensile Strength, YieldElongation at BreakModulus of ElasticityMachinabilityElectrical ResistivityCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting PointSolidusLiquidusAnnealing TemperatureHot-Working TemperatureRecrystallization Temperature
 | 
 | 
 |  | | 