Copper, UNS C70400, H08 Temper
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: CDA 704 (95/5)
Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by forming, bending and welding. Applications: condensers, evaporators, heat exchangers, ferrules, salt water piping, lithium bromide absorption tubing, shipboard condenser intake systems. Available as flat products and tube.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|