Copper Nickel, UNS C71640 Copper Alloy
Subcategory: Copper Alloy; Nonferrous Metal
Close Analogs: Copper content calculated as remainder.
Material Notes: This alloy is similar to the more common C71500, with higher strength and improved corrosion resistance. Common applications include heat exchangers and condensers.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
|
|
|
|