Chromium-Bearing Copper-Nickel, UNS C71900, Half-Hard Temper
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: Cupronickel with Chromium
Material Notes: Applications: Heat exchanger tubes, tube sheets, water boxes, ferrules, saltwater pipe Test specimen: strip.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Liquidus
- Hot-Working Temperature
|
|
|
|