Nickel silver 65-10, UNS C74500, OSO15, Temper flat products
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: NS103, ISO CuNi10Zn27, CEN CW401J
Material Notes: Excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, drawing, etching, forming and bending, heading and upsetting, roll threading and knurling, shearing, spinning, squeezing, stamping and swaging. Applications: rivets, screws, slide fasteners, optical parts, etching stock, hollow ware, nameplates, platers' bars. Test specimen: flat products - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|