Nickel silver 65-12, UNS C75700, OSO15 Temper sheet or strip
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: NS104, ISO CuNi12Zn24, CEN CW403J
Material Notes: Excellent corrosion resistance. Fabricated by blanking, drawing, etching, forming and bending, heading and upsetting, roll threading and knurling, shearing, spinning, squeezing, stamping and swaging. Applications: slide fasteners, camera parts, optical parts, etching stock, nameplates. Test specimen: sheet or strip - 1mm thickness.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|