Copper, UNS C76200
Subcategory: Copper Alloy; Nonferrous Metal
Material Notes: Good to excellent corrosion resistance. Fabricated by blanking, forming and bending, and shearing. Applications: electrical terminals, contact springs, release brackets, ornamental bits and spurs, optical parts, surgical instruments, electrical contacts. Available as flat products and tube.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |