Beryllium-Copper Casting Alloy 275C, UNS C82800, As-Cast
Subcategory: Copper Alloy; Nonferrous Metal
Key Words: BeCu; beryllium copper 275C, CA 828, FED QQ-C-390, MIL-T-16243, MIL-C-19464 (Class IV), ICI-Cu-2-10786
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Investment, Permanent Mold, Plaster, and Sand. Applications: Bearings and molds for plastic parts. Test specimen: as cast.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Melt Temperature
- Solution Temperature
- Aging Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|