Leaded Red Brass, UNS C83600, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded Red Brass, composition metal, ounce metal, 85-5-5-5, CA 836, AMS 4855, ASTM B30, ASTM B62, ASTM B271, ASTM B505, ASTM B584, ASTM B145-4A, SAE J462 (CA836), Ingot code number 115, FED QQ-C-390 (CA836), MIL-C-15345 (Alloy 1)
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, and Sand. Applications: Valves, flanges, pipe fittings, plumbing goods, pump castings, water pump impellers and housings, ornamental fixtures small gears. Classified under: Red Brasses and leaded red brasses. ASTM B62, ASTM B584; formerly ASTM B145-4A As cast values below are for sand casting. Alloy does not respond to heat treating. Casting shrinkage allowance is 5.7%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Creep Strength
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Izod Impact
- Fatigue Strength
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|