Hydraulic Bronze, UNS C83800, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded Red Brass, hydraulic bronze, 83-4-6-7, CA 838, ASTM B30 (CA838), ASTM B271, ASTM B505, ASTM B584, ASTM B145-4B, SAE J462, Ingot code no. 120, FED QQ-C-390
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand. Applications: Low pressure valves and fittings, plumbing supplies and fittings, general hardware, air-gas-water fittings, pump components, railroad catenary fittings. Classified under: Red Brasses and leaded red brasses. ASTM B584; formerly ASTM B145-4B As cast values below are for sand casting. Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Izod Impact
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|