Leaded Yellow Brass, UNS C85400, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded yellow brass, No. 1 yellow brass, 67-1-3-29, CA 854, ASTM B30 (CA854), ASTM B271, ASTM B584; ASTM B146-6B, SAE J462, Ingot code no. 400, FED QQ-C-390, MIL-C-15345 (Alloy 23)
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand. Applications: General purpose yellow casting alloy not subject to high internal pressure. Furniture hardware, ornamental castings, radiator fittings, ship trimmings, cocks, battery clamps, valves and fittings. Classified under: Yellow brasses and leaded yellow brasses. ASTM B584; formerly ASTM B146-6B As cast values below are for sand casting. Alloy does not respond to heat treating. Casting shrinkage allowance is 1.5 - 1.8%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|