Leaded Yellow Brass, UNS C85800, Copper Casting Alloy, Die Castings
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: leaded yellow brass, 63-1-1-35, CA 858, ASTM B30, ASTM B176 (CA858), ASTM B176, ASTM Z30A, SAE J462, Ingot code no. 406, MIL-C-15345 (Alloy 3)
Material Notes:
Casting methods recommended for this alloy: Die. Applications: General purpose die casting alloy having moderate strength. Classified under: Yellow brasses and leaded yellow brasses. ASTM B176; formerly ASTM Z30A Typical data for die castings, separately cast test bars.. Alloy does not respond to heat treating. Casting shrinkage allowance is 2%
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|