Manganese Bronze, UNS C86200, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: High Strength Manganese Bronze, high strength yellow brass, CA 862, ASTM B30, ASTM B271, ASTM B505, ASTM B584; ASTM B147-8B, FED QQ-C-390, FED QQ-C-523, MIL-C-22087 (composition 9), MIL-C-11866 (composition 20), MIL-C-22229 (composition 9), Ingot code no. 423
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Continuous, Die, Investment, Permanent Mold, and Sand. Applications: Marine castings, gears, gun mounts, bushings and bearings. Classified under: Manganese and leaded manganese bronze alloys. ASTM B584; formerly ASTM B147-8B As cast values below are for sand casting. Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Izod Impact
- Machinability
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|