Manganese Bronze, UNS C86300, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: High Strength Manganese Bronze, ASTM B22; ASTM B584; ASTM B22-E; ASTM B147-8C
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Investment, Plaster, and Sand. Applications: Extra heavy duty, high strength alloy. Large valve stems, gears, cams, slow-speed heavy-load bearings, screwdown nuts hydraulic cylinder parts. Classified under: Manganese and leaded manganese bronze alloys. ASTM B22; ASTM B584; formerly ASTM B22-E; ASTM B147-8C As cast values below are for sand casting. Alloy does not respond to heat treating. Casting shrinkage allowance is 2.3%
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
- Electrical Resistivity
- Melting Point
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|