Leaded High-Strength Yellow Brass, UNS C86400, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded Manganese Bronze, ASTM B584; ASTM B147-7A, ASTM B132-A
Material Notes:
Casting methods recommended for this alloy: Centrifugal, Die, Permanent Mold, Plaster, and Sand. Applications: Free machining manganese bronze valve stems, marine fittings, lever arms, brackets, light-duty gears. Classified under: Manganese and leaded manganese bronze alloys. ASTM B584; formerly ASTM B147-7A, ASTM B132-A As cast values below are for sand casting. Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact
- Izod Impact
- Machinability
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|