Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy
Subcategory: Copper Alloy; Nonferrous Metal; Copper Casting Alloy
Key Words: Leaded Manganese Bronze, ASTM B584; ASTM B132-B
Material Notes:
Casting methods recommended for this alloy: Centrifugal and Sand. Applications: High strength free-machining manganese bronze. Valve stems. Classified under: Manganese and leaded manganese bronze alloys. ASTM B584; formerly ASTM B132-B Data typical for as-sand-cast separately cast test bar (M01 temper). Alloy does not respond to heat treating
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Machinability
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|